Edges that are folded or rolled, and the threads and fasteners that go into thin sheet.
HEMS / FOLDED EDGES
Folded edges
A hem stiffens an edge and hides the sharp cut. It needs dedicated tooling, so check availability before designing one in.
View E · closed hemNTS · EM
Material
t (mm)
Min. leg H
L1
L2
Min. Ri
Steel, galv.
1.0
17.0
6
13
0.2
–
1.25
15.5
6
13
0.25
–
1.5
14.8
6
13
0.3
–
2.0
14.0
6
13
0.4
Aluminium
1.0 to 2.0
17.0 to 14.0
6
13
0.2 to 0.4
Stainless
1.0
18.0
6
13
0.2
–
1.25
16.0
6
13
0.25
–
1.5
15.0
6
13
0.3
247TailorSteel, closed hems only, mm. Hemming can mark or crack the surface.
Open hem: inside Ø ≥ t, flange ≥ 4·t Xometry
Tear-drop hem: inside Ø = t, flange ≥ 4·t Xometry
Avoid closed hems on painted or coated stainless and aluminium Xometry
Curl outside radius ≥ 2·t Xometry
Hole clearance from a curl ≥ curl radius + t Xometry
Curl to other bends ≥ 6·t + curl radius Xometry
HARDWARE / THREADS
Tapped holes, countersinks and press-in fasteners
Thread
Core Ø
Min. t
Steel N2
Steel O2
Stainless
Aluminium
M3
2.5
1.0
4
6
5
4
M4
3.3
1.4
4
6
12
4
M5
4.2
1.6
5
6
15
6
M6
5.0
2.0
6
8
20
8
M8
6.8
2.4
8
15
20
8
M10
8.5
3.0
8
15
20
10
M12
10.2
3.0
8
15
20
10
247TailorSteel thread tapping, mm; the last four columns are the maximum sheet thickness. Draw the hole at core Ø and tick it as tapped in Sophia®. Max part 1000 × 1000 or 2000 × 500 mm, 40 kg.
Below the minimum thickness for a tapped thread, use a press-in nut or a weld nut
Countersink depth ≤ 0.6·t, ≥ 8·t between countersinks, 90° for metric screws Xometry
Keep PEM nuts, studs and flanged holes away from the bend region and clear of the tools PCBWay
Install hardware after bending when the bend would load or damage it PCBWay
Send us a sheet metal part before it goes out for quotation. We check it against these rules and the supplier you plan to use, and redesign it where it pays: lighter, stiffer or cheaper to make.